Articles
  • Preparation and chromatic performance of black ceramic tiles from chromium slag, copper slag and silicon manganese slag
  • Yanglai Houa, Jiajie Yua, Dingli Zhengb,c,*, Ju Xub,c, Guojun Mab,c, Shokhrukh Khojievd,e and Nodir Kadirovd,e

  • aCollege of Science, Wuhan University of Science and Technology, Wuhan 430081, Hubei, China
    bKey Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, Hubei, China
    cJoint International Research Laboratory of Refractories and Metallurgy, Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, China
    d“Magistr” private scientific and production enterprise, Tashkent 100106, Republic of Uzbekistan
    eDepartment of Metallurgy, Almalyk branch of Tashkent State Technical University, Tashkent 110100, Republic of Uzbekistan

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. Y.J. Tian, C.Q. Yan, Z.L. Cheng, X.J. Quan, and G. Li, Inorg. Chem. Ind. 53[12] (2021) 129-134.
  •  
  • 2. Z.F. Tong, C.C. Xu, J.X. Wang, and Z.H. Jia, J. Ceram. Process. Res. 24[1] (2023) 17-28.
  •  
  • 3. Z.B. Liu, J.Y. Zheng, W.Z. Liu, X.M. Liu, Y.X. Chen, X.Q. Ren, P. Ning, and Z. Lin, Sci. Total. Environ. 703(2020) 135075.
  •  
  • 4. C.L. Wu, H. Zhang, P.J. He, and L.M. Shao, J. Environ. Sci. 22[7] (2010) 1110-1115.
  •  
  • 5. X.J. Quan, H.Q. Tan, Y.C. Zhao, and Y. Hu, J. Hazard. Mat. 137[2] (2006) 836-841.
  •  
  • 6. Q. Qi, L. Li, L.Y. Wei, B.M. Hu, Z. Liu, and X.Q. Liu, Main. Group. Chem. 20[3] (2021) 317-329.
  •  
  • 7. X. Yan, J.L. Wang, M.J. Zhang, and X.Y. Liu, Chin. J. Biotechno. 37[10] (2021) 3591-3603.
  •  
  • 8. S.H. Huang, B. Peng, Z.H. Yang, L.Y. Chai, and L.C. Zhou, T. Nonferr. Metal. Soc. 19[1] (2009) 241-248.
  •  
  • 9. W.D. Xue, J. Xie, Y. Li, and J.L. Sun, Rare. Metal. Mat. Eng. 38[z2] (2009) 1226-1228.
  •  
  • 10. T. Sun, L.L. Liu, S.Y. Xu, L.L. Wang W. Li, and H. Hao, Micro. Nano. Lett. 8[9] (2013) 487-490.
  •  
  • 11. C.W. Hong, J. Lee, and J.H. Ryu, J. Ceram. Process. Res. 18[4] (2017) 324-328.
  •  
  • 12. T. Kundu, S. Senapati, S.K. Das, S.I. Angadi, and S.S. Rath, Powder Technol.426(2023) 118693.
  •  
  • 13. Y.L. Ye, L.Q. Luo, R.S. Chen, M.X. Wang, C. Liu, and Y.M. Lei, Bull. Chin. Ceram. Soc. 42[5] (2023) 1740-1749.
  •  
  • 14. X.Y. Zhao, T. Yang, J.C. Yang, and Y. Li, Nonferr. Metal. Sci. Eng.14[1] (2023) 99-106.
  •  
  • 15. H.Y. Tian, Z.Q. Guo, J. Pan, D.Q. Zhu, C.C. Yang, Y.X. Xue, S.W. Li, and D.Z. Wang, Resour. Conserv. Recy. 168(2021) 105366.
  •  
  • 16. X.Y. Li, Y. Tang, W.D. Pan, H.M. Shen, X. Chen, Z.Y. Lu, and J. Li, Bull. Chin. Ceram. Soc. 42[5] (2023) 1794-1803.
  •  
  • 17. X.W. Miao, Z.T. Bai, G.H. Lu, L. Liu, M. Gou, F.Q. Cheng, and M. Zhang, Chin. J. Eng. 42[6] (2020) 663-679.
  •  
  • 18. Z.Q. Wang, C. Ma, and C.T. Han, Glass Enamel. 29[6] (2001) 16-18.
  •  
  • 19. L.R. Dou, China's Manganese Industry. 35[4] (2017) 136-138.
  •  
  • 20. X. Xin, Z.X. Tan, J.X. Zhao, A.L. Hu, Z. Wang, Y. Kang, H. Wang, and Z.K. Zhang, J. Chin. Ceram. Soc. 50[6] (2022) 1677-1684.
  •  
  • 21. B. Tanisan and S. Turan, J. Ceram. Process. Res. 12[4] (2011) 462-467.
  •  
  • 22. X. Zhang, Z.Q. Li, G.J. Ma, Q. Wang, and M.K. Liu, Bull. Chin. Ceram. Soc.40[4] (2021) 1318-1329.
  •  
  • 23. G. Costa, V. Della, M. Ribeiro, A. Oliveira, G. Monros, and J. Labrincha, Dyes. Pigments.77[1] (2008) 137-144.
  •  
  • 24. Z.T. Chen, Y. Du, Z.F. Li, D.D. Sun, and C.F. Zhu, Ceram. Int. 41[8] (2015) 9455-9460.
  •  
  • 25. I. S. Vilarinho, J. Carneiro, C. Pinto, J.A. Labrincha, and M.P. Seabra, Sustainability. 13[4] (2021) 1-13.
  •  
  • 26. W. Qin, Z.C. Xu, and H.X. Tian, Foshan. Ceramics,18[2] (2008) 17-20.
  •  
  • 27. K. Chen, C.M. Ke, and J.H. Zhang, J. Wuhan. University. Sci. Techno. 38[5] (2015) 346-350.
  •  
  • 28. H.Q. Ji, P.C. Yan, Discussion on the leaching method of the (Solid Waste-Extraction Procedure for Leaching Toxicity-Sulfuric Acid & Nitric Acid Method). Pollution Control Technology. 2017.
  •  
  • 29. M.K. Liu, G.J. Ma, X. Zhang, D.L. Zheng, and Z.Q. Li, Mater. Today. Commun. 33(2022) 104609.
  •  
  • 30. W.L. Zhang, China Ceramics. 33[5] (1997) 12-14.
  •  
  • 31. B. Gorai and R.K. Jana, Resour. Conserv. Recy. 39[4] (2003) 299-313.
  •  
  • 32. Ceramic Tiles, GB/T4100-2006. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China: Beijing, China, 2006.
  •  
  • 33. Identification Standards for Hazardous Wastes-Identification for Extraction Toxicity. GB 5085.3-2007. General Administration of Quality Supervision, Inspection and Quarantine of the People’s Republic of China: Beijing. China, 2007.
  •  

This Article

  • 2025; 26(1): 139-147

    Published on Feb 28, 2025

  • 10.36410/jcpr.2025.26.1.139
  • Received on Jul 24, 2024
  • Revised on Sep 30, 2024
  • Accepted on Oct 24, 2024

Correspondence to

  • Dingli Zheng
  • bKey Laboratory for Ferrous Metallurgy and Resources Utilization of Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, Hubei, China
    cJoint International Research Laboratory of Refractories and Metallurgy, Ministry of Education, Wuhan University of Science and Technology, Wuhan 430081, China
    Tel : +86-17801024415 Fax: +86-02768862529

  • E-mail: dinglizheng@wust.edu.cn