  • Analysis and preventive measures for spangle formation in antiveiling photoelectric glass
  • Ke Wanga, Meilun Zhanga, Zhenbo Caoa,b,*, Shengyun Yanga, Yu Hana, Qiao Wanga,b, Shaohua Lia, Yang Zhanga,b, Haifeng Lva, You Zhoua,b and Jinsheng Jiaa,b

  • aChina National Building Material Photonics Technology Co., Ltd., Zaozhuang, Shandong, 277000, PR China
    bChina Building Materials Academy Co., Ltd., Beijing, 100000, PR China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. S. Konoshita, F. Sato, S. Yoshihara, and A. Sakamoto, Opt. Mater. 34[4] (2012) 600-603.
  •  
  • 2. M. Kubliha, V. Trnovcová, I. Furár, M. Kadlečíková, J. Pedlíková, and J. Greguš, J. Non-cryst. Solids 355[37-42] (2009) 2035-2039.
  •  
  • 3. J.H. Campbell, J.S. Hayden, and A. Marker, Int. J. Appl. Glass Sci. 2[1] (2011) 3-29.
  •  
  • 4. G.E. Rindone and J.L. Rhoads, J. Am. Ceram. Soc. 39[5] (1956) 173-180.
  •  
  • 5. R.J. Landry and J.T. Fournier, Office. of. Naval. Research, Washington, DC (1969).
  •  
  • 6. C. Wiraseranee, T. Yoshikawa, T.H. Okabe, and K. Morita, Mater. Trans. 55[7] (2014) 1083-1090.
  •  
  • 7. S.N. Li and G.L. Jin, J. Metall. 01 (1982) 581-587.
  •  
  • 8. R.J. Ginther, J. Non-cryst. Solids 6[4] (1971) 294-306.
  •  
  • 9. Y.H. Wang, X.D. Xu, C.K. Zu, K. He, and P. Zhou, J. Funct. Mater. 48[03] (2017) 3078-3082.
  •  
  • 10. S.N. Li and G.L. Jin, J. Non-cryst. Solids 52[1-3] (1982) 47-52.
  •  
  • 11. T. Ha and S. Kang, J. Ceram. Process. Res. 23[2] (2022) 237-242.
  •  
  • 12. X.L. Lv, China Building Materials 08 (2016) 80-81.
  •  
  • 13. D. Kim and S. Kang, J. Ceram. Process. Res. 24[6] (2023) 926-934.
  •  
  • 14. W. Xie, X.S. Jiang, J.N. Xu, Y. Zhou, and D. Wang, J. Vib. Shock 37[24] (2018) 201-207.
  •  
  • 15. H. Li, Y. Han, H. Zhao, W. Qi, D. Zhang, Y. Yu, W. Cai, S. Li, J. Lai, B. Huang, and L. Wang, Nat. Commun. 11[1] (2020) 5437.
  •  
  • 16. K. Li, X. Lv, Z. Li, J. Zheng, Y. Sun, Z. Bo, T. Bo, S. Hong, Z. Kong, T. Na, and C. Wang, AOPC. 11567 (2020) 932-938.
  •  
  • 17. D. Shiratori, Y. Isokawa, H. Samizo, M. Koshimizu, N. Kawaguchi, and T. Yanagida, J. Ceram. Process. Res. 20[4] (2019) 301-306.
  •  
  • 18. L.F. Wang and M.Y. Zhao, in “Optical Glass Technology” (Beijing: Ordnance Industry Press, 1995) p. 98.
  •  
  • 19. M. Hujova and M. Vernerova, Ceram. -Silik. 61[2] (2017) 119-126.
  •  
  • 20. M. Zhang and Y.F. Ma, Glass 50[01] (2023) 30-38.
  •  

This Article

  • 2024; 25(4): 607-612

    Published on Aug 31, 2024

  • 10.36410/jcpr.2024.25.4.607
  • Received on Mar 16, 2024
  • Revised on Jul 18, 2024
  • Accepted on Jul 18, 2024

Correspondence to

  • Zhenbo Cao
  • aChina National Building Material Photonics Technology Co., Ltd., Zaozhuang, Shandong, 277000, PR China
    bChina Building Materials Academy Co., Ltd., Beijing, 100000, PR China
    Tel : 0632-3026007 Fax: 0632-3026006

  • E-mail: czb824@163.com