  • Effect of hydrofluoric acid chemical corrosion on the grinding of silicon nitride ceramic ball
  • Ziqiang Gea, Songhua Lia,b,*, Yuhou Wua,b, Yong Shaa, Jian Suna and Junxing Tiana

  • aSchool of Mechanical Engineering, Shenyang Jianzhu University, Shenyang 110168, China
    bNational-Local Joint Engineering Laboratory of NC Machining Equipment and Technology of High-Grade Stone, Shenyang 110168, China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. L.T. Wei, Y.H. Yu, and J. Jiao, J. Ceram. Process. Res. 19[2] (2018) 126-129.
  •  
  • 2. Y. Lu, J.F. Yang, and J.Q. Gao, J. Ceram. Process. Res. 9[6] (2008) 657-660.
  •  
  • 3. S.H. Ahn and K.W. Nam, J. Ceram. Process. Res. 22[1] (2021) 54-60.
  •  
  • 4. G. Levesque, and N.K. Arakere, Int. J. Solids Struct. 45[25-26] (2008) 6301-6315.
  •  
  • 5. Y.H. Wu, S.H. Li, and K. Zhang, Key Eng. Mater. 291-292 (2005).
  •  
  • 6. T. Kurobe, H. Kakuta, and M. Onoda, J. Jpn. Soc. Precis. Eng. 62[12] (1996) 1773-1777.
  •  
  • 7. B.H. Lv, J.L. Yuan, F. Cheng, and F. Yang, Adv. Mater. Res. doi: 10.4028/www.scientific.net/AMR. 69-70 (2009) 69-73.
  •  
  • 8. N. Umehara, T. Kirtane, R. Gerlick, V.K. Jain, and R. Komanduri, Int. Mach. Tool. Manu. 46[2] (2006) 151-169.
  •  
  • 9. T.H.C. Childs, S. Mahmood, and H.J. Yoon, Tribol. Int. 28[6] (1995) 341-348.
  •  
  • 10. B.H. Lv, J.L. Yuan, Y.X. Yao, and Z.W. Wang, Mater. Sci. Forum. 532 (2006) 460-463.
  •  
  • 11. K.R. Mikeska, S.J. Bennison, and S.L. Grise, J. Am. Ceram. Soc. 83[5] (2000) 1160-1164.
  •  
  • 12. H. Klemm, J. Am. Ceram. Soc. 93[6] (2010) 1501-1522.
  •  
  • 13. M. Herrmann, J. Schilm, W. Hermel, and A. Michaelis, J. Ceram. Soc. Jpn. 114[1335] (2006) 1069-1075.
  •  
  • 14. J. Schilm, M. Herrmann, and G. Michael, J. Eur. Ceram. Soc. 24[8] (2004) 2319-2327.
  •  
  • 15. M. Herrmann, J. Am. Ceram. Soc. 96[10] (2013) 3009-3022.
  •  
  • 16. A.H. Oh, H.S. Lee, B.G. Kim, S.C. Choi, Y.G. Jung, and G.S. An, J. Ceram. Process. Res. 21[4] (2020) 400-406.
  •  
  • 17. S.C. Jeong, S.H. Ahn, and K.W. Nam, J. Ceram. Process. Res. 18[7] (2017) 506-520.
  •  
  • 18. J.R. Frade and M. Cable, J. Mater. Sci. 32[10] (1997) 2727-2733.
  •  
  • 19. M. Herrmann and J. Schilm, Ceram. Int. 35[2] (2009) 797-802.
  •  
  • 20. R. Conradt, J. Am. Ceram. Soc. 91[3] (2008) 728-735.
  •  
  • 21. G.A.C.M. Spierings and J. van Dijk, J. Mater. Sci. 22[5] (1987) 1869-1874.
  •  
  • 22. J.R. Frade and M. Cable, J. Am. Ceram. Soc. 78[1] (1995) 90-96.
  •  
  • 23. T.A. Michalske and S.W. Freiman, J. Am. Ceram. Soc. 66[4] (1983) 284-288.
  •  
  • 24. M. Herrmann, J. Schilm, G. Michael, J. Meinhardt, and R. Flegler, J. Eur. Ceram. Soc. 23[4] (2003) 585-594.
  •  
  • 25. J. Schilm, M. Herrmann, and G. Michael, J. Eur. Ceram. Soc. 27[12] (2007) 3573-3588.
  •  
  • 26. B. Seipel and K.G. Nickel, Ceram. Int. 30[2] (2004) 267-271.
  •  
  • 27. T. Sato, Y. Tokunaga, T. Endo, M. Shimada, K. Komeya, K. Nishida, and T. Kameda, J. Mater. Sci. 23[10] (1988) 3440-3446.
  •  
  • 28. S.W. Sharkawy and A.M. El-Aslabi, Corros. Sci. 40[7] (1998) 1119-1129.
  •  
  • 29. J.H. Gong, in “Fracture mechanics of ceramics” (Beijing: Tsinghua University Press, 2001).
  •  

This Article

  • 2022; 23(5): 685-693

    Published on Oct 31, 2022

  • 10.36410/jcpr.2022.23.5.685
  • Received on Apr 7, 2022
  • Revised on Jun 24, 2022
  • Accepted on Jun 25, 2022

Correspondence to

  • Songhua Li
  • aSchool of Mechanical Engineering, Shenyang Jianzhu University, Shenyang 110168, China
    bNational-Local Joint Engineering Laboratory of NC Machining Equipment and Technology of High-Grade Stone, Shenyang 110168, China
    Tel : +86-24-24694319 Fax: +86-24-24694319

  • E-mail: lisonghua@sjzu.edu.cn