Articles
  • Bending strength and wear characteristics of Si3N4 composites containing additives SiO2 and TiO2
  • Seok-Hwan Ahna and Ki-Woo Namb,*

  • aDepartment of Aero Mechanical Engineering, Jungwon University, Chungbuk 28024, Korea
    bDepartment of Materials Science and Engineering, Pukyong National University, Busan 48547, Korea

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. F.F. Lange, J. Am. Ceram. Soc. 53[5] (1970) 290.
  •  
  • 2. E.A. Gulbransen and S.A. Jansson, Oxid. Met. 4[3] (1972) 181-201.
  •  
  • 3. J.J. Petrovic and L.A. Jacobson, J. Am. Ceram. Soc. 59[1–2] (1976) 34-37.
  •  
  • 4. T.K. Gupta, J. Am. Ceram. Soc. 59[5-6] (1976) 259-262.
  •  
  • 5. J. Korouš, M.C. Chu, M. Nakatani, and K. Ando, J. Am. Ceram. Soc. 83[11] (2000) 2788-2792.
  •  
  • 6. T. Osada, W. Nakao, K. Takahashi, K. Ando, and S. Saito, J. Eur. Ceram. Soc. 27[10] (2007) 3261-3267.
  •  
  • 7. K.H. Kang and J.D. Yun, J. Ceram. Process. Res. 12[5] (2011) 583-587.
  •  
  • 8. Y.T. Kim, S.G. Kim, and J.W. Park, J. Ceram. Process. Res. 16[5] (2015) 624-628.
  •  
  • 9. P.S. Lee, T.H. Ahn, S.H. Kim, H.M. Kim, and K.B. Shim, J. Ceram. Process. Res. 16[S1] (2015) 114-131.
  •  
  • 10. Y.S. Jung, Y. Guo, W. Nakao, K. Takahashi, K. Ando, and S. Saito, Fatigue Fract. Engng. Mater. Struct. 31[1] (2008) 2-11.
  •  
  • 11. K.W. Nam, H.R. Jeong, J.W. Kim, and S.H Ahn, J. Ceram. Process. Res. 17[11] (2016) 1188-1191.
  •  
  • 12. K.H. Lee, K.W. Nam, and S.H. Ahn, J. Ceram. Process. Res. 18[12] (2017) 831-842.
  •  
  • 13. H.S. Nam, J. Ceram. Process. Res. 20[4] (2019) 379-387.
  •  
  • 14. J.W. Lee, K.W. Nam, and W. Nakao, J. Ceram. Process. Res. 21[2] (2020) 200-207.
  •  
  • 15. K.W. Nam, S.W. Park, J.Y. Do, and S.H. Ahn, Trans. of KSME, A 32[11] (2008) 957-962.
  •  
  • 16. K.W. Nam, J. Powder Tech. 2013 (2013) 695895.
  •  
  • 17. K.W. Nam and J.S. Kim, Mater. Sci. Eng. A 527[13-14] (2010) 3236-3239.
  •  
  • 18. F. Tavangarian, D. Hui, and G. Li, Engineering 144 (2018) 56-87.
  •  
  • 19. H.J. Yang, Y.T. Pei, J.C. Rao, J.Th.M. De Hosson, S.B. Li, and G.M. Song, Scripta Materialia 65[2] (2011) 135-138.
  •  
  • 20. K.W. Nam and J.R. Hwang, J. Mech. Sci. Tech. 26[7] (2011) 2093-2096.
  •  
  • 21. K.W. Nam, M.K. Kim, S.W. Park, S.H. Ahn, and J.S. Kim (2007), Mater. Sci. Eng. A 471[1-2] (2007) 102-105.
  •  
  • 22. K.W Nam, J.S. Kim, and S.W. Park, Int. J. Mod. Phys. B 24[15-16] (2010) 2869-2874.
  •  
  • 23. K. Ando, K. Houjyou, M.C. Chu, S. Takeshita, K. Takahashi, S. Sakamoto, and S. Sato, J. Eur. Ceram. Soc. 22[8] (2002) 1339-1346.
  •  
  • 24. K.W. Nam S.H. Park, and J.S. Kim, J. Ceram. Process. Res. 10[4] (2009) 497-501.
  •  
  • 25. S.K. Lee, W. Ishida, S.Y. Lee, K.W. Nam, and K. Ando, J. Eur. Ceram. Soc. 25[5] (2005) 569-576.
  •  
  • 26. D. Jianxin, Ceram. Int. 27[2] (2001) 135-141.
  •  
  • 27. N. Vashishth, S.G. Sapate, P. Bagde, and A.B. Rathod, Tribol. Int. 118 (2018) 381-399.
  •  
  • 28. K.J. Siczek, in “Tribological processes in the valve train systems with lightweight valves: New research and modelling” (Butterworth-Heinemann, 2016) pp. 85-180.
  •  
  • 29. K.W. Nam and J.S. Kim, J. Ceram. Process. Res. 11[1] (2010) 20-24.
  •  
  • 30. M.K. Kim, H.S. Kim, S.B. Kang, S.H. Ahn, and K.W. Nam, Solid State Phenomena. 124-126 (2007) 719-722.
  •  

This Article

  • 2021; 22(1): 54-60

    Published on Feb 28, 2021

  • 10.36410/jcpr.2021.22.1.54
  • Received on Jun 26, 2020
  • Revised on Jul 16, 2020
  • Accepted on Aug 14, 2020

Correspondence to

  • Ki-Woo Nam
  • Department of Materials Science and Engineering, Pukyong National University, Busan 48547, Korea
    Tel : +82-51-629-6358 Fax: +82-51-629-6353

  • E-mail: namkw@pknu.ac.kr