Articles
  • Mechanical properties of silicon carbide/graphene nanoplatelets composites prepared by spark plasma sintering
  • Zhang Xiulinga, Chen Yuhonga,b,*, Liu Limenga, Qi Wubina, Hai Wanxiua,b, Xue Mina and Hong Tianxianga

  • aSchool of Materials Science and Engineering, North Minzu University, Yinchuan, 750021, China
    bKey Lab of Powder Material & Advanced Ceramics, Yinchuan 750021, China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. S. Li, X.D. Luo, C.C. Wei, P.L. Gao, P. Wang, and L.J. Zhou, J. Alloys. Compd. 834 (2020) 155252.
  •  
  • 2. D. Sciti and A. Bellosi, J. Mater. Sci. 35[15] (2000) 3849-3855.
  •  
  • 3. Y. Cao, R.Y. Deng, J.L. Hu, J.X. He, D.P. Lei, Z.J. Chen, and Y.X. Peng, J. Ceram. Process. Res. 24[2] (2023) 321-328.
  •  
  • 4. C.G. Lee, X.D. Wei, J.W. Kysar, and J. Hone, Sci. 321[5887] (2008) 385-388.
  •  
  • 5. A. Nieto, A. Bisht, D. Lahiri, C. Zhang, and A. Agarwal, Int. Mater. Rev. 62[5] (2016) 241-302.
  •  
  • 6. I.-J. Shon, Ceram. Process. Res. 17[11] (2016) 1171-1174.
  •  
  • 7. C. Chen, X.C. Han, H.H. Shen, Y.Q. Tan, H.B. Zhang, Y. Qin, and S.M. Peng, Ceram. Int. 46[14] (2020) 23173-23179.
  •  
  • 8. M. Nader, F. Aldinger, and M. Hoffmann, J. Mater. Sci. 34[6] (1999) 1197-1204.
  •  
  • 9. T. Maruyama, Y. Yamashita, T. Saida, S.-I. Tanaka, and S. Naritsuka, J. Cryst. Growth. 468 (2017) 175-178.
  •  
  • 10. A.N. Manuel Belmonte, Pierre Boutbien, Benito Román-Manso, María I. Osendi, Pilar Miranzo, Scripta. Mater. 113 (2016) 127-130.
  •  
  • 11. P. Miranzo, C. Ramírez, B. Román-Manso, L. Garzón, H. Gutiérrez, M. Terrones, C. Ocal, M.I. Osendi, and M. Belmonte, J. Eur. Ceram. Soc. 33[10] (2013) 1665-1674.
  •  
  • 12. Q.S. Li, Y.J. Zhang, H.Y Gong, H.B. Sun, W.J. Li, L. Ma, and Y.S. Zhang, J. Mater. Sci. Technol. 32[7] (2016) 633-638.
  •  
  • 13. E. Bódis, I. Cora, C. Balázsi, P. Németh, Z. Károly, S. Klébert, P. Fazekas, A.M. Keszler, and J. Szépvölgyi, Ceram. Int. 43[12] (2017) 9005-9011.
  •  
  • 14. J.M. Anna Kaźmierczak-Bałata, Ceram. Int. 44[9] (2018) 10273-10280.
  •  
  • 15. X.Z. Guo, R. Wang, P. Zheng, Z.J. Lu, and H. Yang, Adv. Appl. Ceram. 118[7] (2019) 409-417.
  •  
  • 16. R. Sedlák, A. Kovalŀíková, V. Girman, E. Múdra, P. Rutkowski, A. Dubiel, and J. Dusza, J. Eur. Ceram. Soc. 37[14] (2017) 4307-4314.
  •  
  • 17. N. Lu, J.X. Liu, G. He, and J.T. Li, Solid. State. Phenom. 281 (2018) 125-130.
  •  
  • 18. A. Eckmann, A. Felten, A. Mishchenko, L. Britnell, R. Krupke, K.S. Novoselov, and C. Casiraghi, Nano. Lett. 12[8] (2012) 3925-3930.
  •  
  • 19. J.Z Zhun, Y.M. Shang, and Y. Liu, Petrochemical. Technology. 51[11] (2022) 1323-1329.
  •  
  • 20. B. Zhang, T.J. Chen, L.Y. Wang, and B.Q. Yang, J. Funct. Mater. 50[08] (2019) 8133-8139.
  •  
  • 21. V.-H. Nguyen, S.A. Delbari, M. Shahedi Asl, Q.V. Le, A. Sabahi Namini, Z. Ahmadi, M. Farvizi, M. Mohammadi, and M. Shokouhimehr, Ceram. Int. 47[9] (2021) 12459-12466.
  •  
  • 22. C. López-Pernía, Á. Gallardo-López, A. Morales-Rodríguez, and R. Poyato, J. Eur. Ceram. Soc. 39[14] (2019) 4435-4439.
  •  
  • 23. L.X. Liu, Y. Wang, X.H. Li, L. Xu, X.X. Cao, Y.H. Wang, Z.G. Wang, C.M. Meng, W.J. Zhu, and X.P Ouyang, J. Am. Ceram. Soc. 99[1] (2016) 257-264.
  •  
  • 24. M. Balog, J. Kečkéš, T. Schöberl, D. Galusek, F. Hofer, J. Křesťan, Z. Lenčéš, J.-L. Huang, and P. Šajgalík, J. Eur. Ceram. Soc. 27[5] (2007) 2145-2152.
  •  
  • 25. C. Yun, Y. Feng, T. Qiu, J. Yang, X. Li, and L. Yu, Ceram. Int. 41[7] (2015) 8643-8649.
  •  
  • 26. Y.H. Huang, D.L. Jiang, X.F. Zhang, Z.K. Liao, and Z.R. Huang, J. Eur. Ceram. Soc. 38[13] (2018) 4329-4337.
  •  
  • 27. Z.Y.B. Zeng, Y.Z. Liu, W.P. Chen, X.Q. Li, Q.F. Zheng, K.L. Li, and R.R. Guo, J. Am. Ceram. Soc. 101[8] (2018) 3498-3507.
  •  
  • 28. J.H. Gong, J. Adv. Ceram. 42 (2021) 287-428.
  •  
  • 29. A. Nieto, D. Lahiri, and A. Agarwal, Mat. Sci. Eng. A-Struct. 582 (2013) 338-346.
  •  
  • 30. B. Lanfant, Y. Leconte, G. Bonnefont, V. Garnier, Y. Jorand, S. Le Gallet, M. Pinault, N. Herlin-Boime, F. Bernard, and G. Fantozzi, J. Eur. Ceram. Soc. 35[13] (2015) 3369-3379.
  •  

This Article

  • 2024; 25(4): 483-489

    Published on Aug 31, 2024

  • 10.36410/jcpr.2024.25.4.483
  • Received on Sep 12, 2023
  • Revised on Nov 23, 2023
  • Accepted on Dec 4, 2023

Correspondence to

  • Chen Yuhong
  • aSchool of Materials Science and Engineering, North Minzu University, Yinchuan, 750021, China
    bKey Lab of Powder Material & Advanced Ceramics, Yinchuan 750021, China
    Tel : 13079598519 Fax: 0086-951-2066827

  • E-mail: lyhchen@163.com