Articles
  • Experimental investigation on the dielectric and impedance properties of indium doped titanium dioxide ceramics
  • Liqi Cui, Ruifeng Niu, Depeng Wang and Weitian Wang*

  • School of Physics and Electronic Information, Yantai University, Yantai 264005, P.R. China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. C. Moure and O. Peña, Prog. Solid State Chem. 43[4] (2015) 123-148.
  •  
  • 2. C. Pecharromán, F. Esteban‐Betegón, J. Bartolomé, S. López‐Esteban, and J. Moya, Adv. Mater. 13[20] (2001) 1541-1544.
  •  
  • 3. O. Thakur, C. Prakash, and D. Agrawal, J. Ceram. Process. Res. 3[2] (2002) 75-79.
  •  
  • 4. X.-G. Zhao, P. Liu, Y.-C. Song, A.-P. Zhang, X.-M. Chen, and J.-P. Zhou, Phys. Chem. Chem. Phys. 17[35] (2015) 23132-23139.
  •  
  • 5. R. Islam, S. Choudhury, S. Rahman, and M.J. Rahman, J. Ceram. Process. Res. 13[3] (2012) 248-251.
  •  
  • 6. S. Yasmin, S. Choudhury, M. Hakim, A. Bhuiyan, and M. Rahman, J. Ceram. Process. Res. 12[4] (2011) 387-391.
  •  
  • 7. X.W. Wang, P.B. Jia, X.E. Wang, B.H. Zhang, L.Y. Sun, and Q.B. Liu, J. Mater. Sci.: Mater. Electron. 27[11] (2016) 12134-12140.
  •  
  • 8. W. Zhou, M. Cao, H. Wang, H. Hao, Z. Yao, and H. Liu, Ceram. Int. 48[12] (2022) 16723-16729.
  •  
  • 9. L. Cui, R. Niu, and W. Wang, J. Ceram. Process. Res. 23[1] (2022) 57-61.
  •  
  • 10. W. Hu, Y. Liu, R.L. Withers, T.J. Frankcombe, L. Norén, A. Snashall, M. Kitchin, P. Smith, B. Gong, H. Chen, J. Schiemer, F. Brink, and J. Wong-Leung, Nat. Mater. 12[9] (2013) 821-826.
  •  
  • 11. Z. Wang, H. Chen, W. Nian, J. Fan, Y. Li, and X. Wang, J. Alloys Compd. 777 (2019) 317-324.
  •  
  • 12. S. Chao and F. Dogan, J. Am. Ceram. Soc. 94[1] (2011) 179-186.
  •  
  • 13. H.H. Nguyena, G. Gyawali, and B. Joshi, J. Ceram. Process. Res. 23[1] (2022) 33-40.
  •  
  • 14. F. Peng and D. Zhu, Ceram. Int. 44[17] (2018) 21034-21039.
  •  
  • 15. Y. Yu, W.-L. Li, Y. Zhao, T.-D. Zhang, R.-X. Song, Y.-L. Zhang, Z.-Y. Wang, and W.-D. Fei, J. Eur. Ceram. Soc. 38[4] (2018) 1576-1582.
  •  
  • 16. Z. Cao, J. Zhao, and J. Fan, Ceram. Int. 47[5] (2021) 6711-6719.
  •  
  • 17. H.M. Albetran and I.M. Low, Arab. J. Chem. 13[2] (2020) 3946-3956.
  •  
  • 18. C. Zhao, Z. Li, and J. Wu, J. Mater. Chem. C 7[14] (2019) 4235-4243.
  •  
  • 19. M. Khan, Z. Lan, and Y. Zeng, Materials 11[6] (2018) 952.
  •  
  • 20. T. Ji, Y. Gao, T. Qin, D. Yue, H. Liu, Y. Han, and C. Gao, J. Phys. Chem. C 125[6] (2021) 3314-3319.
  •  
  • 21. P. Anithakumari, B.P. Mandal, S. Nigam, C. Majumder, M. Mohapatra, and A.K. Tyagi, New J. Chem. 41[21] (2017) 13067-13075.
  •  
  • 22. P. Kumar, A.K. Sharma, B.P. Singh, T.P. Sinha, and N.K. Singh, Physica B 403[1] (2010) 103-108.
  •  
  • 23. A.K. Jonscher, Dielectric Relaxation in Solids (Chelsea Dielectrics, London, 1983).
  •  
  • 24. A.K. Jonscher, Nature 267[5613] (1977) 673-679.
  •  
  • 25. Q. Wang, O. Varghese, C.A. Grimes, and E.C. Dickey, Solid State Ionics 178[3] (2007) 187-194.
  •  
  • 26. X. Guo and J. Maier, J. Electrochem. Soc. 148[3] (2001) E121.
  •  
  • 27. D.C. Sinclair and A.R. West, J. Mater. Sci. 29[23] (1994) 6061-6068.
  •  

This Article

  • 2023; 24(2): 348-352

    Published on Apr 30, 2023

  • 10.36410/jcpr.2023.24.2.348
  • Received on Nov 17, 2022
  • Revised on Jan 19, 2023
  • Accepted on Jan 27, 2023

Correspondence to

  • Weitian Wang
  • School of Physics and Electronic Information, Yantai University, Yantai 264005, P.R. China
    Tel : +86 13573512787 Fax: +86 535 6901947

  • E-mail: wtwang@ytu.edu.cn