  • Preparation of decorative slag glass-ceramics and research on the solidification of heavy metals
  • Yang Tanga, Xiaodong Haoa, Zhenxiang Fanga, Xinyu Baia, Guangyu Wanga, Hongxia Zhanga, Leibo Denga, Hua Chena,b, Ming Zhaob and Yongsheng Dua,b,*

  • aCollege of Science, Inner Mongolia University of Science and Technology, Baotou 014010, China
    bCollaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources, Inner Mongolia University of Science and Technology, Baotou 014010, China

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. G.H. Ai, Y.F. Liu, Y. Wang, and Y.L. Chen, J. Residuals Sci. Tech. 12[1] (2015) 17-23.
  •  
  • 2. B. Wang, X.Y. Yuan, L. Han, X.Y. Wang, and L.J. Zhang, Environ. Earth Sci. 74[6] (2015) 5087-5096.
  •  
  • 3. X.H. Chen, H.X. Guo, and X.H. Cheng, Environ. Geotech. 5[2] (2018) 107-113.
  •  
  • 4. T. Chen, C. Lei, B. Yan, L.L. Li, D.M. Xu, and G.G. Ying, Environ. Sci. Pollut. R. 25[36] (2018) 36702-36711.
  •  
  • 5. B.W. Li, L.B. Deng, X.F. Zhang, and X.L. Jia, J. Non-Cryst. Solids 380 (2013) 103-108.
  •  
  • 6. Y.L. Zhao, J.P. Qiu, M.A. Zhengyu, Z.B. Guo, and H. Liu, Powder Technol. 375 (2020) 539-548.
  •  
  • 7. H. Park, Y. Jeong, Y.B. Jun and J.E. Oh, Constr Build Mater. 122 (2016) 343-353.
  •  
  • 8. G.B. Wang, Q.Q. Zhang, W.C. Du, R.Z. Lin, J.H. Li, F.X. Ai, Y. Yin, R. Ji, X.R. Wang, and H.Y. Guo, Ecotoxicol Environ Saf. 207 (2021) 111275.
  •  
  • 9. W.C. Ma, D.M. Chen, M.H. Pan, T.B. Gu, L. Zhong, G.Y. Chen, B.B. Yan, and Z.J. Cheng, J. Environ. Manage. 247 (2019) 169-177.
  •  
  • 10. J.G. Jiang, J. Wang, X. Xu, W. Wang, Z. Deng, and Y. Zhang, J. Hazard. Mater. 113[1-3] (2004) 141-146.
  •  
  • 11. Y.L. Pi, W.H. Zhang, Y.S. Zhang, W.T. Zou, Z.X. Zhang, and F. Wu, Ceram. Int. 47[17] (2021) 24663-24674.
  •  
  • 12. B.Q. Li, Y.P. Guo, and J.Z. Fang, J. Alloy. Compd. 881 (2021) 159821.
  •  
  • 13. L. Liu, Y.L. Li, and Z.K. Zhang, J. Clean. Prod. 269 (2020) 122417.
  •  
  • 14. S.Z. Zhao, Q. Wen, X.Y. Zhang, B. Liu, and S.G. Zhang, Ceram. Int. 47[15] (2021) 21599-21609.
  •  
  • 15. C. Li, Q. Wen, M. Hong, Z. Liang, Z. Zhuang, and Y. Yu, Constr. Build. Mater. 134 (2017) 443-451.
  •  
  • 16. Y.L. Pi, W.H. Zhang, Y.S. Zhang, W.T. Zou, Z.X. Zhang, and F. Wu, Ceram. Int. 47[17] (2021) 24663-24674.
  •  
  • 17. L.Y. Tang, R.H. Han, and J. Quan, J. Wuhan Univ. Technol. 34[6] (2012) 6-9.
  •  
  • 18. H. Yang and X.Z. Guo, Int. J. Mater. Prod. Tec. 37[3-4] (2010) 280-286.
  •  
  • 19. T. Suzuki, K. Horibuchi, and Y. Ohishi, J. Non-Cryst. Solids 351[27-29] (2005) 2304-2309.
  •  
  • 20. J.W. Xue, J.W. Zhong, Y.R. Mao, C.H. Xu, W. Liu, and Y.Q. Huang, Ceram. Int. 46 (2020) 23186-23193.
  •  
  • 21. G.Y. Wang, Y.S. Du, J. Ma, H.X. Zhang, S.L. Ouyang, L.B. Deng, H. Chen, and M. Zhao, J. Ceram. Process. Res. 22[6] (2021) 665-674.
  •  
  • 22. S.A.M. Abdel-Hameed, M.A. Marzouk, and A.E. Abdel-Ghany, J. Non-Cryst. Solids 357[24] (2011) 3888-3896.
  •  
  • 23. H.A. Elbatal, Z.S. Mandouh, H.A. Zayed, S.Y. Marzouk, G.M. Elkomy, and A. Hosny, J. Non-Cryst. Solids 358 (2012) 1806-1813.
  •  
  • 24. E.M.A. Hamzawy and C. Leonelli, Glass Technol. 46[3] (2005) 281-286.
  •  
  • 25. H.X. Zheng, M.W. Colby, and J.D. Mackenzie, J. Non-Cryst. Solids, 127[2] (1991) 143-150.
  •  
  • 26. H.R. Li, S.Y. Liu, W.C. Xu, Y.X. Zhang, Y. Shi, J. Ma, S.L. Ouyang, and Y.S. Du, J. Eur. Ceram. Soc. 41[2] (2021) 1603-1612.
  •  
  • 27. H. Chen, B. W.Li, M. Zhao, X.F. Zhang, Y.S. Du, Y. Shi, and J.S. McCloy, J. Non-Cryst. Solids 524 (2019) 119638.
  •  
  • 28. S.L. Ouyang, Y.X. Zhang, Y.X. Chen, Z.W. Zhao, M. Wen, B.W. Li, Y. Shi, M.Z. Zhang, and S.L. Liu, Sci. Rep. 9 (2019) 1964.
  •  
  • 29. J. Ma, Y. Shi, H.X. Zhang, S.L. Ouyang, L.B. Deng, H. Chen, M. Zhao, and Y.S. Du, Mater. Chem. Phys. 261 (2021) 124213.
  •  
  • 30. M.V.S. Rao, S. Suresh, T. Narendrudu, A.S. Kumar, G.C. Ram, and D.K. Rao, J. Mol. Struct. 1125 (2016) 624-632.
  •  
  • 31. H.X. Zhang, Y.S. Du, X.W. Yang, X.F. Zhang, M. Zhao, H. Chen, S.L. Ouyang, and B.W. Li, J. Non-Cryst. Solids, 482 (2018) 105-115.
  •  
  • 32. G.X. Gayo and A.E. Lavat, Ceram. Int. 44[18] (2018) 22181-22188.
  •  
  • 33. T.M. Gross, J. Lahiri, A. Golas, J. Luo, F. Verrier, J.L. Kurzejewski, D.E. Baker, J. Wang, P.F. Novak, and M.J. Snyder, Nat. Commun. 10 (2019) 1979.
  •  
  • 34. X. Chen, T.C. Chadwick, R.M. Wilson, R. Hill, and M.J. Cattell, J. Dent. Res. 89[12] (2010) 1510-1516.
  •  
  • 35. D.D. Feng, Y.M. Zhu, F.F. Li, and Z.H. Li, J. Eur. Ceram. Soc. 36[10] (2016) 2579-2585.
  •  
  • 36. W. Dang and H.Y. He, J. Ceram. Process. Res. 21[1] (2020) 69-74.
  •  
  • 37. W.T. Zou, W.H. Zhang, Y.L. Pi, Y.S. Zhang, L. Zhang, and Y. Chen, Ceram Int. 48 (2022) 5040-5053.
  •  
  • 38. C.H. Li, W. Zhao, J.L. Zhang, W. Lu, P. Li, B.J. Yan, and H.W. Guo, J. Ceram. Process. Res. 22[4] (2021) 409-420.
  •  
  • 39. N. Gao, Y.X. Chen, C.G. Wang, Y.L. Guo, and J.Y. Zhang, J. Ceram. Process. Res. 22[6] (2021) 714-721.
  •  

This Article

  • 2023; 24(1): 58-68

    Published on Feb 28, 2023

  • 10.36410/jcpr.2023.24.1.58
  • Received on Jun 14, 2022
  • Revised on Aug 17, 2022
  • Accepted on Sep 3, 2022

Correspondence to

  • Yongsheng Du
  • aCollege of Science, Inner Mongolia University of Science and Technology, Baotou 014010, China
    bCollaborative Innovation Center of Integrated Exploitation of Bayan Obo Multi-Metal Resources, Inner Mongolia University of Science and Technology, Baotou 014010, China
    Tel : +86-472-5954358 Fax: +86-472-5954358

  • E-mail: dys1111@imust.edu.cn