Articles
  • X-ray diffraction and raman spectroscopy studies on calcium modified PZT (Pb(1-x)CaxZr0.52Ti0.48O3) ceramics prepared via solid state reaction method and sol-gel technique- a comparative study
  • Anupama Sachdevaa,*, Aarushib, Jagneet Kaur Ananda and R.P. Tandonc

  • aKeshav Mahavidyalaya, University of Delhi, Delhi 110034, India
    bDepartment of Electrical Engineering, Texas A&M University, College Station, Texas 77840, USA
    cDepartment of Physics and Astrophysics, University of Delhi, Delhi 110007, India

  • This article is an open access article distributed under the terms of the Creative Commons Attribution Non-Commercial License (http://creativecommons.org/licenses/by-nc/4.0) which permits unrestricted non-commercial use, distribution, and reproduction in any medium, provided the original work is properly cited.

References
  • 1. B. Jaffe, W.R. Cook, and H. Jaffe, in “Piezoelectric Ceramics” (Academic Press, 1971).
  •  
  • 2. Y. Xu, in “Ferroelectric Materials and Their Applications” (Elsevier Science, 2013).
  •  
  • 3. N.F.K. Bahanurddin, M.H. Jumali, J.J. Mohamed, and Z.A. Ahmad, J. Ceram. Process. Res. 16[2] (2015) 258-261.
  •  
  • 4. S.K. Sinha, A.K. Sinha, P. Kour, and P.K. Barhai, J. Ceram. Process. Res. 12[1] (2011) 93-95.
  •  
  • 5. A. Ari-gur and L. Benguigui, Solid State Commun. 15[6] (1974) 1077-1079.
  •  
  • 6. K. Kakegawa, J. Mohri, K. Takahasi, H. Yamamura, and S. Shirasaki, Solid State Commun. 24[11] (1977) 769-772.
  •  
  • 7. K. Kakegawa, J. Mohri, S. Shirasaki, and K. Takahasi, J. Am. Ceram. Soc. 65[10] (1982) 515-519.
  •  
  • 8. W. Cao and L.E. Cross, Phys. Rev. B. 47[9] (1993) 4825-4830.
  •  
  • 9. A.P. Singh, S.K. Mishra, R. Lal, and D. Pandey, Ferroelectrics. 163[1] (1995) 103-113.
  •  
  • 10. K. Kakegawa, O. Matsunaga, T. Kato, and Y. Sasaki, J. Am. Ceram. Soc. 78[4] (1995) 1071-1075.
  •  
  • 11. J.C. Fernandes, D.A. Hall, M.R. Cockburn, and G.N. Greaves, Nucl. Instrum. Methods Phys. Res. B. 97[1-4] (1995) 137-141.
  •  
  • 12. S.K. Mishra, A.P. Singh, and D. Pandey, Appl. Phys. Lett. 69[12] (1996) 1707-1709.
  •  
  • 13. E.R. Leite, M. Cequeira, L.A. Perzaoli, R.S. Nasar, E. Longo, and J.A. Varela, J. Am. Ceram. Soc. 79[6] (1996) 1563-1568.
  •  
  • 14. Ragini, R. Ranjan, S.K. Mishra, and D. Pandey, J. Appl. Phys. 92[6] (2002) 3266-3274.
  •  
  • 15. Y. Ishibashi, and M. Iwata, Jpn. J. Appl. Phys. 37[8B] (1998) L985-L987.
  •  
  • 16. X. Du, J. Zheng, U. Belegundu, and K. Uchino, Appl. Phys. Lett. 72[19] (1998) 2421-2423.
  •  
  • 17. B. Noheda, Curr. Opin. Solid State Mater. Sci. 6[1] (2002) 27-34.
  •  
  • 18. B. Noheda, D.E. Cox, G. Shirane, J.A. Gonzalo, L.E. Cross, and S.-E. Park, Appl. Phys. Lett. 74[14] (1999) 2059.
  •  
  • 19. B. Noheda, J.A. Gonzalo, R. Guo, S.-E. Park, L.E. Cross, D.E. Cox, and G. Shirane, Phys. Rev. B. 61[13] (2000) 8687-8695.
  •  
  • 20. L. Bellaiche, A. Garcia, and D. Vanderbilt, Phys. Rev. Lett. 84[23] (2000) 5427-5430.
  •  
  • 21. D. Vanderbilt, and M.H. Cohen Phys. Rev. B. 63[9] (2001) 094108(1-9).
  •  
  • 22. B. Noheda, D.E. Cox, G. Shirane, R. Guo, B. Jones, and L.E. Cross, Phys. Rev. B. 63[1] (2000) 014103(1-9).
  •  
  • 23. K.C.V. Lima, A.G. Souza Filho, A.P. Ayala, J. Mendes Filho, P.T.C. Freire, F.E.A. Melo, E.B. Araújo, and J.A. Eiras, Phys. Rev. B. 63[18] (2001) 184105 (1-5).
  •  
  • 24. A.K. Singh, D. Pandey, S. Yoon, S. Baik, and N. Shin, Appl. Phys. Lett. 91[19] (2007) 192904(1-3).
  •  
  • 25. X.Q. Ke, D. Wang, X. Ren, and Y. Wang, Phys. Rev. B. 88[21] (2013) 214105(1-6).
  •  
  • 26. R.S. Solanki, S.K. Mishra, A. Senyshyn, S. Yoon, S. Baik, N. Shin, and D. Pandey, Appl. Phys. Lett. 102[5] (2013) 052903(1-5).
  •  
  • 27. F. Cordero, Materials 8[12] (2015) 8195-8245.
  •  
  • 28. L. Fan, J. Chen, Y. Ren, Z. Pan, L. Zhang, and X. Xing, Phys. Rev. Lett. 116[2] (2016) 027601(1-5).
  •  
  • 29. J. Zhao, S.D. Funni, E.R. Molina, E.C. Dickey, and J.L. Jones, J. Euro. Ceram. Soc. 41[6] (2021) 3357-3362.
  •  
  • 30. A. Sachdeva, V. Luthra, P. Gautam, and R.P. Tandon, Integr. Ferroelectr. 122[1] (2010) 74-82.
  •  
  • 31. A. Sachdeva, Aarushi, J.K. Anand, and R.P. Tandon, J. Ceram. Process. Res. 23[1] (2022) 99-108.
  •  
  • 32. A. Beitollahi, J. Mater. Sci. 38[6] (2003) 1219-1229.
  •  
  • 33. H. Huang, Z. Tianshu, J.T. Oh, and P. Hing, Ferroelectrics. 274[1] (2002) 55-65.
  •  
  • 34. A. Boutarfaia, C. Boudaren, A. Mousser, and S.E. Bouaoud, Ceram. Int. 21[6] (1995) 391-394.
  •  
  • 35. H. Chen, J. Long, and Z. Meng, Mater. Sci. Eng. B. 99[1-3] (2003) 433-436.
  •  
  • 36. C. Dong, J. Appl. Cryst. 32[4] (1999) 838-838.
  •  
  • 37. H. Miura, J. Crystallogr. Soc. Jpn. 45[2] (2003) 145-147.
  •  
  • 38. A.G. Souza Filho, K.C.V. Lima, A.P. Ayala, I. Guedes, P.T.C. Freire, F.E.A. Melo, J. Mendes Filho, E.B. Araújo, and J.A. Eiras, Phys. Rev. B. 66[13] (2002) 132107(1-4).
  •  
  • 39. H. Zhang, S. Leppävuori, and P. Karjalainen, J. Appl. Phys. 77[6] (1995) 2691-2696.
  •  
  • 40. J.F. Meng, R.S. Katiyar, G.T. Zou, and X.H. Wang, Phys. Stat. Sol. 164[2] (1997) 851-862.
  •  
  • 41. P.S. Dobel and R.S. Katiyar, J. Raman Spectrosc. 33[6] (2002) 405-423.
  •  
  • 42. S.R. Shannigrahi and S. Tripathy, Ceram. Int. 33[4] (2007) 595-600.
  •  
  • 43. H. Zhang, A. Uusimäki, S. Leppävuori, and P. Karjalainen, J. Appl. Phys. 76[7] (1994) 4294-4300.
  •  

This Article

  • 2022; 23(6): 817-822

    Published on Dec 31, 2022

  • 10.36410/jcpr.2022.23.6.817
  • Received on Mar 30, 2022
  • Revised on Jul 2, 2022
  • Accepted on Jul 23, 2022

Correspondence to

  • Anupama Sachdeva
  • Keshav Mahavidyalaya, University of Delhi, Delhi 110034, India
    Tel : +91-11-47083152 Fax: +91-11-47083152

  • E-mail: anupama_sachdeva@hotmail.com